Sign In | Join Free | My polstate.com
China DONGGUAN LONROY EQUIPMENT CO LTD logo
DONGGUAN LONROY EQUIPMENT CO LTD
DONGGUAN LONROY EQUIPMENT CO LTD
Verified Supplier

2 Years

Home > Thermal Analyzer >

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument

DONGGUAN LONROY EQUIPMENT CO LTD
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument

Type : Testing Machine

MOQ : 1

Protection Class : Ip56

customized support : OEM, ODM, OBM

Voltage : 220 V

Accuracy : /

warranty : 1 Year

Accuracy Class : High Accuracy

Brand Name : LONROY

Application : Auto Testing

power : ---

Place of Origin : Guangdong, China

Contact Now

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument

Product Introduction

The LR-DSC-40A is designed based on the tower heat flow principle. It is a conventional thermal analysis instrument that measures the change of the heat flow difference between the sample and the reference sample over time or temperature under program temperature control. This product uses milligram-level sample volume and can measure basic data such as specific heat, glass transition temperature, melting point, melting enthalpy, reaction heat of thermosetting plastics, reaction kinetics of thermosetting plastics, and gelation conversion rate.

Test standards

GB/T 22232, ASTM E2253, GB/T 28724, ASTM E793, GB/T 19466, ASTM E794, GB/T 28723, ASTM E1269, GB/T 13464, JJG 936

Testing characteristics

Thermodynamic and kinetic analysis

Application fields

Polymer materials | Biomedicine | New materials | Petrochemicals | New energy

Product features

1. Using mature tower-type heat flow technology, the instrument's resolution and sensitivity are enhanced.

2. High-performance heat flow sensors with antioxidant substrates are adopted to achieve higher sensitivity and better dynamic response, accurately capturing micro-temperature changes.

3. The silver furnace body ensures higher heat transfer efficiency and reduces cross-interference between reference and sample.

4. The instrument has heating and isothermal control modes.

5. The instrument has analysis functions such as DSC Onset Point, Start set Point, Endset Point, baseline, heat flow peak, glass transition temperature, heat peak area, heat absorption and release enthalpy, peak temperature, extrapolated temperature, specific heat, etc.

6. The data acquisition frequency of the instrument reaches 50Hz, effectively enhancing the instrument's sensitivity and resolution.

7. The optimized structural design provides reliable baseline stability for the instrument and improves the signal-to-noise ratio.

8. A high-definition touch screen is configured, enabling quick and easy operation of the instrument.

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument

Technical Specification

Temperature control range

RT~700℃

Temperature control mode

Temperature rise, constant temperature (RT-400℃)

Heating rate

(0.05~200)℃/min

Heating rate deviation

Better than 1%

Cooling method

Air cooling

Phase transition temperature precision

±0.02℃ (In)

Phase transition temperature accuracy

±0.1℃ (In)

Baseline stability

≤100μW (100~300℃, no deduction)

Baseline repeatability

≤40μW

Heat flow peak noise

Better than 8μW

Enthalpy measurement precision

±0.08% (In)

Enthalpy measurement accuracy

±0.8% (In)

Indium peak height / half peak width

≥20.0mW/K

TAWN resolution

R(20)≤0.3

TAWN sensitivity

S(0.1)≥3

Sampling frequency

50Hz

Heat flow measurement range

±750mW

Gas path module

3-channel gas path control, inert/oxidizing atmosphere, static/dynamic mode, 0~300mL/min

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis InstrumentLONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis InstrumentLONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis InstrumentLONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument


Product Tags:

ASTM E2253 differential scanning calorimeter

      

tower heat flow thermal analyzer

      

ASTM E794 thermal analysis instrument

      
Wholesale LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument from china suppliers

LONROY ASTM E2253 ASTM E793 Differential Scanning Calorimeter ASTM E794 ASTM E1269 Tower Heat Flow Thermal Analysis Instrument Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: DONGGUAN LONROY EQUIPMENT CO LTD
*Subject:
*Message:
Characters Remaining: (0/3000)